3Dプリントの公差 — 完璧な嵌合と組み立てを実現するための設計

This 3d printing tolerances design guide explains practical considerations for material selection, design review, manufacturing, and sourcing decisions.

Designing parts that fit together is one of the biggest challenges in functional 3D printing. This guide covers tolerance principles, testing methods, and design strategies for perfect assemblies.

3Dプリントの公差 — 完璧な嵌合と組み立てを実現するための設計

Understanding Tolerances

Tolerance is the intentional dimensional deviation from nominal size that allows parts to fit together. In 3D printing, tolerances account for:

  • Material shrinkage: ABS shrinks more than PLA
  • Nozzle size: Wider nozzles = larger minimum features
  • 層の高さ: Affects vertical dimensions
  • Machine accuracy: Varies between printers

生産用途 require consistent tolerances.

3D Printing Tolerances — Designing for Perfect Fit and Assembly - testing

Standard Tolerances by Fit Type

Press Fit (Interference)

目的: Permanent or semi-permanent connection

素材 おすすめ
PLA -0.15 to -0.25mm
PETG -0.20 to -0.30mm
ABS/ASA -0.25 to -0.35mm
ナイロン -0.30 to -0.40mm
TPU -0.40 to -0.60mm

Sliding Fit (Clearance)

目的: Parts that move relative to each other

用途 Clearance
Light slide +0.10 to +0.15mm
Free slide +0.20 to +0.30mm
Loose fit +0.30 to +0.50mm

Wrench/Screw Fit

目的: Tool engagement

Tool Size おすすめ
<5mm +0.20mm
5-10mm +0.30mm
>10mm +0.40mm
3D Printing Tolerances — Designing for Perfect Fit and Assembly - applications

Tolerance Testing

Calibration Cube Method

Print a standard tolerance test:

1. Download a tolerance test model (multiple size holes/pins)
2. Print with your standard settings
3. Test fit with go/no-go gauges
4. Adjust design based on results

Temperature affects tolerances — calibrate at working temperature.

Material-Specific Testing

Different materials require different approaches:

PLA/PETG: Stable, consistent tolerances
ABS/ASA: Account for shrinkage (0.3-0.5%)
ナイロン: Largest variance, test thoroughly
TPU: Compression affects measurements

Design Strategies

Horizontal Holes

  • Standard holes print undersized
  • Add +0.2 to +0.4mm to nominal
  • Consider vertical orientation for accuracy

Vertical Holes

  • More accurate than horizontal
  • Add +0.1 to +0.2mm to nominal
  • Top layers affect diameter

Pins and Shafts

  • Print at nominal or slightly undersized
  • Vertical orientation most accurate
  • Sand to final dimension if needed

Higher infill improves dimensional stability.

Assembly Techniques

Snap Fit Design

Parameters:

  • Cantilever length: 4-6x thickness
  • Thickness: 1-2mm typical
  • Engagement: 0.5-1.0mm

Thread Design

  • Avoid printed threads for strength applications
  • Use threaded inserts for better holding power
  • Design holes for insert interference fit

Living Hinges

  • Works best with flexible materials (TPU, PETG)
  • Minimum thickness: 0.4mm
  • Hinge length affects flexibility

よくあるご質問

When is 3D Printing Tolerances — Designing for Perfect Fit and Assembly a good option?

3D Printing Tolerances — Designing for Perfect Fit and Assembly is a good option when fast iteration, complex geometry, low tooling cost, or low-volume production is more important than molded-part unit cost.

What should be checked before choosing 3D Printing Tolerances — Designing for Perfect Fit and Assembly?

部品サイズ、材料特性、表面仕上げ、寸法公差、熱暴露、荷重方向、後処理が必要かどうかを確認する。.

How does 3D Printing Tolerances — Designing for Perfect Fit and Assembly compare with CNC machining?

3Dプリンティングは複雑な形状を素早く作ることができるが、CNC機械加工は精密な表面、より厳しい公差、生産グレードの材料に強いことが多い。.

What affects the cost of 3D Printing Tolerances — Designing for Perfect Fit and Assembly?

コストは、材料、造形量、印刷時間、レイヤーの高さ、サポート除去、仕上げ、検査、造形物の部品数によって異なる。.

ご使用の部品について教えてください

このフィールドは必須です。.
このフィールドは必須です。.
このフィールドは必須です。.
このフィールドは必須です。.
このフィールドは必須です。.
このフィールドは必須です。.
このフィールドは必須です。.

関連記事

。
トップに戻る