PA6 GF GB30: ガラス繊維とガラスビーズ強化ナイロン6の完全ガイド

PA6 GF GB30 usually refers to a PA6 molding compound with both chopped glass fiber and glass beads. Buyers compare it with fiber-only PA6 when a molded cover, enclosure or locating feature needs stiffness together with controlled warpage. Confirm the producer’s designation, the glass split and the actual part requirements before ordering.

Compounded resin pellets beside a molded connector housing concept
Illustrative compounded pellets and housing. Check the supplier’s actual formulation and grade designation.

PA6 GF GB30とは何ですか?

GF denotes glass fiber and GB denotes glass beads. For example, BASF identifies Ultramid B3GK24 Uncolored as PA6-(GF+GB)30, a combined glass-fiber and glass-bead reinforced molding grade. In that designation, 30 identifies the combined filler loading by mass. It does not specify bead diameter or the split between fibers and beads. Confirm how the producer of the quoted grade uses its code.

当社のエンジニアリングプラスチックの供給について

For a resin enquiry, provide the required formulation, color, quantity and application. For a molded part, include the drawing and the defect or fit problem you are trying to solve. Request documents for the actual supplier, grade and production location where applicable.

ガラスビーズとガラス繊維の補強効果の違い

Schematic contrasting elongated glass fibers and spherical glass beads
Filler shapes shown schematically. Size and fiber-to-bead ratio depend on the exact compound.
Filler Typical role What to request
Chopped glass fiber Stiffens the compound, with reinforcement influenced by flow direction Mechanical data in relevant directions and evidence at critical weld lines
Glass beads A spherical filler that can alter the shrinkage balance of a formulation Flow and transverse shrinkage values and molded-part flatness
Glass fiber plus glass beads Lets the producer tune a balance of stiffness and dimensional behavior Exact grade and filler breakdown if available, plus actual-part molding results

What Can a Hybrid Grade Improve?

Mating molded enclosure halves on an inspection fixture
Review mating gap and flatness after conditioning on a representative enclosure. Illustrative setup.

A hybrid grade is worth testing when the fiber-only baseline meets load requirements but leaves a warped sealing face, uneven seam or cosmetic problem. Spherical beads have no long axis, but fibers in the same compound still orient with flow. Gate location, packing, cooling and wall layout also affect final shape.

Compare samples in the same tool under agreed molding and conditioning states. Record flatness, mating gap, visible surface, impact and load performance. Gloss, injection pressure and cycle time require their own checks.

機械的特性、熱的特性、および寸法特性

プロパティ 比較するための証拠
Stiffness, strength and impact Current TDS for the quoted compound, with test method, conditioning and orientation
HDT and heat aging Test load and specimen conditions for HDT, then retained properties under the actual duty cycle
Shrinkage, CLTE and fit Flow and transverse values with measurement conditions, plus dimensions after relevant conditioning
表面品質 A molded sample with the intended gate, color and surface texture

比較:PA6 GF30 対 PA6 GF GB30 対 PA6 GB30

Grade strategy When to evaluate it Decision evidence
PA6 GF30 Load-bearing baseline with about 30% glass fiber when specified by the supplier Confirm strength and stiffness in the load direction and check warp around interfaces
PA6 GB30 Bead-filled candidate when appearance or fit dominates Confirm bead loading, impact and the load capacity of the actual part
PA6-(GF+GB)30 Hybrid candidate when the existing grade has a measurable flatness or assembly issue Compare two grade samples against the same dimensional, cosmetic and mechanical criteria

代表的なアプリケーション

Molded sensor housing concepts and a separate perimeter gasket
Illustrative cover and seal interface. Review flatness, gasket compression and relevant exposure before approval.

Consider a hybrid compound for covers, locator features and multi-piece housings where distortion changes the assembled gap. Separate a cosmetic cover from a pressure-carrying, high-heat or electrically rated part. The latter needs its own fluid, heat-aging, pressure or electrical verification for the exact grade and geometry.

GFおよびGB充填コンパウンドの加工ガイドライン

Open mold concept with a ribbed molded enclosure sample
Illustrative tooling arrangement. Confirm the grade process window, gate and cooling with the toolmaker.

Set drying and residual moisture from the grade instructions. Use the recommended melt and mold windows, then qualify filling, packing and cooling on the actual mold. Check gates, vents, wear surfaces and ejector access with the toolmaker.

Before releasing the material, agree how to compare warp, weld-line performance, assembly fit and appearance. For a part or mold review, send the drawing, annual volume, current material, defect photos and the relevant load and conditioning requirements. Review injection molding options または Request a grade comparison.

よくあるご質問

Does GB30 mean a 30-micrometer glass bead?

No. Check the supplier’s notation. In a designation such as PA6-(GF+GB)30, the 30 identifies the combined filler loading. Bead size and the fiber-to-bead split require separate supplier data.

Will the hybrid grade remove warpage?

It may change the balance of shrinkage. Compare an actual molding in the same tool and verify flatness and fit in the specified conditioning state.

Can PA6-(GF+GB)30 replace PA6 GF30 directly?

Compare the exact grades for strength, impact, shrinkage, moisture response and processing. Confirm the tool and the assembly before approving the substitution.

What should the supplier quote include?

Ask for the grade designation, current TDS, sample quantity and intended molding conditions. Include the drawing, critical datums, annual volume and the failure or defect to resolve.

Tell Us About Your Part

このフィールドは必須です。.
このフィールドは必須です。.
このフィールドは必須です。.
このフィールドは必須です。.
このフィールドは必須です。.
このフィールドは必須です。.
このフィールドは必須です。.

関連記事

なぜナイロンプラスチックを選ぶのか

生産において、剛性、寸法管理、調達リスクのバランスを考慮する必要がある場合、ナイロンプラスチックはPA6強化グレードの採用が推奨されます。.

トップに戻る