ABS CF10 Carbon Fiber Reinforced Pellets

ABS CF10 is a carbon-fiber-reinforced ABS compound supplied as pellets. The reference grade is ABS WHC10A. Evaluate it for molded housings, fixtures and brackets where stiffness, assembly fit and surface appearance need to be considered together.

Reference grade: ABS WHC10A

Supply: 10% carbon fiber reinforced pellets. Confirm color, quantity and required documents with your inquiry.

カテゴリー:

ABS CF10 Material Overview

ABS CF10 is a carbon-fiber-reinforced ABS compound supplied as pellets. The reference grade is ABS WHC10A. Evaluate it for molded housings, fixtures and brackets where stiffness, assembly fit and surface appearance need to be considered together.

項目 詳細
Reference grade ABS WHC10A
Polymer ABS
補強 10% carbon fiber
Form Pellets for material-supply inquiries
Color and processing Confirm the offered grade and current processing guidance

Reference Material Properties

Typical values for ABS WHC10A from the linked supplier PDF.

プロパティ 代表値 試験方法
引張強度 86 MPa ISO 527
曲げ強度 131 MPa ISO 178
曲げ弾性率 9480 MPa ISO 178
Notched impact strength 5.9 kJ/m² ISO 180

Specimen conditioning is not stated in the reference sheet. These values are not guaranteed specification limits. Only rows with a usable property, unit and method are reproduced; request clarification of the remaining sheet entries before relying on them for design.

Download ABS WHC10A supplier reference datasheet (PDF)

Application Review

ABS CF10 illustrative component applications
Illustrative component concepts. Confirm the selected formulation for the actual part.

Instrument enclosures

Review lid fit, ribs, screw bosses and openings around the equipment. Check impact and temperature requirements on molded samples.

Locating fixtures

Define locating faces, hole spacing and clamp loads. Fiber content alone does not establish the accuracy of a finished fixture.

Mounting brackets

Check insert retention, load direction and sustained deflection. Use the actual bracket and fasteners for the assembly trial.

Processing and Part Checks

Confirm drying and processing guidance for WHC10A before molding. Review gate position, fiber orientation, weld lines and visible surfaces. A carbon-filled designation does not establish a particular electrical resistance or ESD classification.

For component production, review our injection molding service. For other resin options, browse engineering plastic materials.

Material Supply and Manufacturing Support

ナイロン・プラスチック connects engineering plastic supply with custom manufacturing. WANHAN is our cooperating compounding factory; the photographs below show its material-feeding equipment, extrusion process and laboratory.

Material feeding equipment at WANHAN, Nylon Plastic’s cooperating factory
Material feeding
Extruded plastic strands at the WANHAN cooperating factory
Extrusion process
Laboratory work area at the WANHAN cooperating factory
Laboratory

Grade and formulation selection

Share your current grade, application and operating conditions. We coordinate the material review and identify the matching datasheet for the formulation offered.

Quality documents for your order

Specify the TDS, batch records, inspection requirements or compliance files your purchasing team needs. The documents and acceptance criteria are agreed for the quoted material.

Support beyond resin pellets

For a finished component, connect material selection with part design, tooling and molding review. Start with the drawing, expected quantity and critical dimensions.

Cooperating Factory Management-System Certificates

The supplied ISO 9001, ISO 14001 and ISO 45001 certificates identify Guangdong Wanhan as the certified entity. Their scope concerns modified plastic granules and the related management activities; it does not certify every material grade or every finished-part manufacturing service.

Review manufacturing capabilities and quality documentation. For document approval, match the legal entity, certificate scope and quoted grade.

よくある質問

What material does this page cover?

ABS CF10 is a carbon-fiber-reinforced ABS compound supplied as pellets. The reference grade is ABS WHC10A. Evaluate it for molded housings, fixtures and brackets where stiffness, assembly fit and surface appearance need to be considered together.

Does ABS CF10 have a confirmed ESD rating?

The reference PDF does not provide a usable electrical-resistance method and unit. No ESD or shielding classification is specified here. Request the relevant test report for the exact grade and component.

Are these values a production specification?

No. They are typical reference values for ABS WHC10A. Agree the current grade, test conditions, acceptance limits and required documents for the order.

Do the images show the exact supplied color and finished parts?

The images illustrate resin appearance and possible component concepts. Confirm color and finish on the offered material and samples; the pictured parts do not establish suitability for your design.

What is required for a material replacement?

Identify the current resin and reason for changing it. Compare exact-grade data, dimensions, loads, temperature and environmental exposure, then validate the intended part before production.

What should I send for a quote or sample request?

Send the reference grade, application, color, estimated material quantity and required documents. For a molded-part inquiry, add the drawing, critical dimensions and acceptance requirements. A CAD file is optional for a material-only inquiry.

Related Material Grades

ABS CF20   |   ABS CF30

Request Material Data and a Quote

Share the grade, application, service conditions, color, quantity and required documents so the offered material can be reviewed against your project.

Request ABS WHC10A TDS and Quote

トップに戻る

連絡先

下記のフォームにご記入ください。.

連絡先